repousee-msg - 5/9/20 Period process or hammering out an object from the backside once the object is stuck to a pitch/plaster mixture in a pitchbowl. NOTE: See also the files: metalworking-msg, metalworking-FAQ, metals-msg, blacksmithing-msg, tools-msg. ************************************************************************ NOTICE - This file is a collection of various messages having a common theme that I have collected from my reading of the various computer networks. Some messages date back to 1989, some may be as recent as yesterday. This file is part of a collection of files called Stefan's Florilegium. These files are available on the Internet at: http://www.florilegium.org I have done a limited amount of editing. Messages having to do with separate topics were sometimes split into different files and sometimes extraneous information was removed. For instance, the message IDs were removed to save space and remove clutter. The comments made in these messages are not necessarily my viewpoints. I make no claims as to the accuracy of the information given by the individual authors. Please respect the time and efforts of those who have written these messages. The copyright status of these messages is unclear at this time. If information is published from these messages, please give credit to the originator(s). Thank you, Mark S. Harris AKA: THLord Stefan li Rous Stefan at florilegium.org ************************************************************************ Date: Tue, 22 Dec 1998 12:17:18 -0500 From: rmhowe To: sca-arts at raven.cc.ukans.edu Subject: Repousee Maggie Allen wrote: > Pardon my ignorance but what is Repousee? The process of hammering metal out from the _backside_ once it has been stuck to a pitch/plaster mixture in a pitchbowl. Chasing is basically touching it up from the front. In either case punches and a hammer are used. It produces raised decorations in sheet metals. They can be flat to begin with or even bowls or raised objects like vases - in which case you might use a snarling iron. Ok, what is a snarling iron? A snarling iron is a double bent piece of steel which sits horizontally out from a vise. One bend goes down into the vise and is held there. The other end goes vertically up and is shaped into whatever is appropriate for the design you wish to raise on the surface of the vessel. One places the vessel over the iron, feels by tipping it a bit where the iron tip is touching and whacks the iron with a hammer, thus causing it to rebound and bump up the surface of the vessel. Once sufficient metal has been raised it is generally refined (chased) by filling the vessel with pitch and hammering the metal back with punches to bring out the detail. Why do you use pitch? You use pitch because it has the ability to hold the metal without deforming it while it has the ability to give under the blows of the punch and hammer. One melts the pitch carefully with a torch and sticks the metal to it - or one melts the pitch in a double boiler and pours it into it. One heats the metal to unstick it or pour it out. One uses a 'soft' flame to heat the metal, not a high temperature torch. One does _not_ heat the pitch from below in an ordinary pan unless one likes being covered with very hot sticky tar. Gases will build up under it. You can also use a bell hammer to beat out the surface in a vessel. A Bell hammer is basically shaped like a P without the straight continuation of the line in front of the curve of the P. It generally has a ball at the end of the curve. One carefully swings it inside the object to raise the surface. You generally still end up chasing the surface. Magnus Date: Mon, 21 Dec 1998 10:32:45 -0800 (PST) From: Heidi Johnson To: sca-arts at raven.cc.ukans.edu Subject: Re: Need Sources for Documenting Repousee ---Gunnora Hallakarva wrote: > A gentleman here in Ansteorra has asked me if I can assist him in locating > sources documenting medieval repousee techniques. Repousee is most definitely period, although without a more specific period reference, I can only give you general information to pass on. Here are a few books that might be helpful: Secondary sources: Anne Garside Ed., Jewelry Ancient to Modern, Viking Press, 1979 G. Gregorietti, Jewelry through the ages, American Heritage Press, New York 1969 T. Hackens, A. Winkes, Gold Jewelry. Craft, Style and Meaning from Mycenae to Constantinopolis, Belgium 1983 H. Hodges, ARTIFACTS An introduction to early materials and technology, Duckworch, London 1989 Jewelry -- 7,000 Years The Trustees of the British Museum © 1986, 1991 Harry Abrams, Inc. Ronald W. Lightbown, Medieval European Jewelry, © Victoria and Albert Museum Tylecote R.F, The early history of metallurgy in Europe, Longman, New York l987 And Primary Sources: Agricola, Georgius De Re Metallica Albertus Magnus, Book of Minerals,Tr. by Dorothy Wyckoff. Oxford 1967 Cellini, Benvenuto, Treatise on Goldsmithing and Sculpture, Tr. by C. R. Ashbee, N. Y. 1967 Theophilus, On Divers Arts, Tr. by J. Hawthorne and C. Smith. Chicago 1976 (Also available in a Dover edition) Kassia Tzykandelina, Nordskogen, Northshield, Midrealm mka Heidi Johnson Date: Wed, 5 May 1999 02:02:56 -0500From: Roberta R Comstock To: sca-arts at raven.cc.ukans.eduSubject: Re: Repousse I haven't done much metalwork myself, but have sure studied a lot of it.My favorite handy (and cheap!) technical reference is _Metalwork &Enamelling_ by Herbert Maryon. 5th Ed. New York: Dover. 1971. ISBN0-486-22702-2There's an excellent book I picked up at the metropolitan in New Yorkabout 15 years ago. Don't have it handy at the moment, but i think thetitle is something like 'The Treasure of San Marco' in Venice. It's abeautifully illustrated catalog of the loot from the sack ofConstantinople. OOdles of reliquaries with repousse icons all over them,ornate book covers, chalices, religious pariphenalia (mostly Christian),etc, etc etc. Mounting varies.There are a lot of period pieces that are copper-gilt or vermeille(which, if i remember right is silver-gilt), and a variety of othermetals and alloys, not always precious metals.Have fun.Hertha Date: Wed, 5 May 1999 15:36:21 -0500 (CDT)From: Lorine S Horvath To: sca-arts at raven.cc.ukans.eduSubject: Re: Repousse On Tue, 4 May 1999 GoodhueMA at aol.com wrote:> Repousse Questions>> Were base metals used and then gilded? If so when?> I don't know. I haven't found examples of gilding in my research yet.Hi! Tarrach here. In answer to the question below: There is asubstantial amount of evidence for guilding on bronze repousse on findsfrom the 7th century. See discussions in The Sutton Hoo Ship Burial:Arms Armour and Regailia by R. Bruce-Mitford (1978). Note, most of thestuff from Sutton Hoo was actual gold, but the repousse helmet plaqueswere of bronze that had been tinned (kind of like guilding in tin).There are some excellent gold gilt bronze repousse work from theValsgard and Vendal finds of the same time period. Hope this helps. Date: Wed, 05 May 1999 17:39:52 -0400From: rmhowe To: sca-arts at raven.cc.ukans.eduSubject: Re: Repousse Lorine S Horvath wrote:> Hi! Tarrach here. In answer to the question below: There is a> substantial amount of evidence for guilding on bronze repousse on finds> >from the 7th century. See discussions in The Sutton Hoo Ship Burial:> Arms Armour and Regailia by R. Bruce-Mitford (1978). Note, most of the> stuff from Sutton Hoo was actual gold, but the repousse helmet plaques> were of bronze that had been tinned (kind of like guilding in tin).> There are some excellent gold gilt bronze repousse work from the> Valsgard and Vendal finds of the same time period. Hope this helps.Note: the plates were most probably made by hammering the metal betweena lead sheet and a bronze matrix with the design cast onto it.Hammering deforms the lead and pushes the metal beneath it down onto the design. I believe there are examples of these kinds of moldsin Viking to Crusader. The original matrix was most probably lost waxcast in a tempered clay mold. This makes for mass production relativelyeasily. You will note that there are more than one identical plate.See:Aspects of AngloSaxon Archaeology, Sutton Hoo and Other Discoveries,by Rupert Bruce Mitford, Keeper of Medieval and Later Antiquitiesin the British Museum, Harpers Magazine Press, New York 1974.ISBN 06 120480 3 LOC 73 13220 Harper and Row Publishers.This book includes detailed articles on the Sutton Hoo Ship Burial,Saxon Rendlesham, The Snape Boat Grave, An earlier Sutton Hooexcavation diary, Later Sutton Hoo excavations, Ship's Figure Headsfrom the Migration Period, The Sutton Hoo Lyre, The Sutton Hoo Helmet,and a new reconstrution of it, The Torslunda Plates (Matrices), TheBenty Grange Helmet and other supposed Anglo Saxon Helmets, S.H. andthe Background of Beowulf, Six interesting pieces of Cloisonne Jewelry,St. Cuthbert's Pectoral Cross, Late Saxon Disc Brooches, and a blueglass jar. The book is fairly specific on most constrution details.The Sutton Hoo Lyre is in detail in all it's pieces.I'm not sure if Thora has used it for her reconstruction or not,but I thought I'd mention it in case she's missed this one. :)I know she has an article on it on her fine webpages.There was a medium grade book written recently with the titleRepousse. It's not bad but it's not great either. Have it but can'tfind it for a citation. Should still be on the market.Magnus Date: Thu, 6 May 1999 20:05:53 -0500 (CDT) From: Lorine S Horvath To: sca-arts at raven.cc.ukans.edu Subject: Re: Repousse > Note: the plates were most probably made by hammering the metal between > a lead sheet and a bronze matrix with the design cast onto it. > Hammering deforms the lead and pushes the metal beneath it down on > to the design. I believe there are examples of these kinds of molds > in Viking to Crusader. The original matrix was most probably lost wax > cast in a tempered clay mold. This makes for mass production relatively > easily. You will note that there are more than one identical plate. Oh! Good point! I guess the helmet plaques probably do not fall into the category of true Repousse. However, it should be noted that some of the shield mounts from Valsgard are not all (or even mostly identical, and are a bit on the long side to have been stamped out. Although, such a comment should be tempered with the possibility that they could have been. See G. Arwidsson: Die Graberfunde von Valsgard I, Valsgard 6 Acta Musei Antiquitatum Septentrionalium Regiae Universitatis IV (1942), Also, similar titles and publisher Valgard II Valsgard 8 (1954). Also, see the close-up of the tail section of the bird shaped shield mount from Sutton Hoo (Figure 44 in Bruce-Mitford Vol. II).This piece (although gold rather than gilt bronze appears to have been done in a true repousse technique. YIS Tarrach From the fb "Artisans of the Society for Creative Anachronism" group: Pedro Bedard August 3 at 10:22pm Cathyn McKenna How did you make the pitch-tray? The wood frame part is pretty self explanatory, but how did you load the pitch? How deep is the pitch itself? Pedro Bedard The pitch was melted, and poured in like hot wax. And, it's about 1/2" deep. You don't need much. Pedro Bedard Emma, yes, this is all my work. Cathryn, let me know how it works for you, I've never tried commercial pitch Jean, I work with sheet between 16 and 22 ga. Whatever I can get at the scrap yard. Cathyn McKenna I'm thinking of using this product: http://www.riogrande.com/.../Medium-Red-Chaser.../118265... Pedro Bedard As I said, I've never used commercially available pitch before. But from its composition, it looks just fine! Ari Anson I get my pitch form http://www.chasers-pitch.com/ John Michael Thorpe that red stuff from Rio is horrible. I tried it because the red pitch is what Valentin Yotkov recommends, I used it once and scrapped it. I use the black from Grobet (what comes in the can when you order the pitch bowl with pitch from Rio) much lower melting temp, gets a little runny at summer tent temperatures, but moves great, and super easy to work, and melts below serious flesh burn temperatures, and dissolves in alcohol, or if you are working outdoors burns off leaving a tiny bit of white ash which wipes off Mark Feldmann I got mine from Northwest Pitchworks, I believe. I got the medium hardness, if I recall. I haven't used it enough to really give a critical report but I like it. I usually use a heat gun rather than a plumber's torch, less smoke. By the way, this is a light gold color and came poured into a reused milk carton. Pedro Bedard I've heard good things about the northwest pitchworks products, but I've never tried them myself. August 5 at 7:08pm Gerald Loosehelm I am using the black from Grobet. It came with my pitch bowl from Rio as well. It sucks! Hard as a rock. you do a little work and it separates from the metal so you are constantly heating the copper to get it to adhere and the pitch be soft enough to move under the copper. I was going to get the northwest pitchworks products but I now regret that I did not. 8/6/15 at 7:00am John Michael Thorpe Gerald are you greasing the metal like you have to with the red and the Northwest product? Gerald Loosehelm I have been using a light coat of mineral oil on the back of my metal. But it is more the pitch. Very hard and brittle. It melts like you said. at a lower temp but it just sucks unless I am constantly heating it slightly. 8/6/15 at 7:14am Gerald Loosehelm Maybe I just got a bad batch. John Michael Thorpe I just put the metal in the pitch. Never have to grease it John Michael Thorpe If the pitch is too hard I give it a slight warming before working with it. Below 70 degrees it is a little hard but a quick pass with a feathered flame a couple of times before working sets it up Gerald Loosehelm For me, below 80 it is a rock. I am wondering if I got a bad batch. John Michael Thorpe Maybe, I tend to warm mine by putting metal on and taking off regularly and am used to just flicking the torch at it if it is too stiff so hard to tell. Lisa Webster Love the photo of you working at your craft! This is something that has called to me for quite some time, but the cost of the tools and materials have made me not take it up yet. You all share such great info though! Thanks for sharing!' 8/7/15 Pedro Bedard Lisa, my wife and I have a rule; if we take up a new hobby, we aren't allowed to spend more than $50.00 trying it out. I started with pitch from work (asphaltum, it stinks but it works) two pans from a goodwill store as pitch pans, an old cobblers hammer I found at a yard sale, and some tools from Princess Auto (Harbor freight, same thing) that I ground and polished myself. That and some scrap brass and copper is what got me going. It really doesn't have to be expensive. Edited by Mark S. Harris respousee-msg Page 2 of 7